Quote:
Originally Posted by kgoerz
I did this one the other Day. Basic Krylon, Brown, Tan and Green.
1. Cleaned entire AR with Break Cleaner. Scrubbed with Soap and Hot Water.
2. Baked it 250 degrees for about thirty minutes.
3. Let Cool, Tape and paint
|
how well does Krylon usually hold up for you? Also are you using the ultra flat stuff that they make for hunting and what not?